TABLA DE REFERENCIAS – LIJAS ABRASIVAS NO ADHESIVAS | ||||
200 Ø TIPO S | 230 Ø TIPO S | 250 Ø TIPO S | 300 Ø TIPO S | |
GRANO | ||||
P-60 | 377013099 | 377013161 | ||
P-100 | 377013100 | 377013110 | 377013120 | 377013130 |
P-120 | 377013101 | 377013111 | 377013121 | 377013131 |
P-180 | 377013102 | 377013112 | 377013122 | 377013132 |
P-240 | 377013103 | 377013113 | 377013123 | 377013133 |
P-320 | 377013104 | 377013114 | 377013124 | 377013134 |
P-400 | 377013105 | 377013115 | 377013125 | 377013135 |
P-600 | 377013106 | 377013116 | 377013126 | 377013136 |
P-800 | 377013107 | 377013117 | 377013127 | 377013137 |
200 Ø TIPO M | 230 Ø TIPO M | 250 Ø TIPO M | 300 Ø TIPO M | |
GRANO | ||||
P-80 | 377013400 | 377013410 | 377013420 | 377013430 |
P-120 | 377013401 | 377013411 | 377013421 | 377013431 |
P-180 | 377013402 | 377013412 | 377013422 | 377013432 |
P-240 | 377013403 | 377013413 | 377013423 | 377013433 |
P-320 | 377013404 | 377013414 | 377013424 | 377013434 |
P-400 | 377013405 | 377013415 | 377013425 | 377013435 |
P-600 | 377013406 | 377013416 | 377013426 | 377013436 |
P-800 | 377013407 | 377013417 | 377013427 | 377013437 |
P-1000 | 377013408 | 377013418 | 377013428 | 377013438 |
P-1200 | 377013409 | 377013419 | 377013429 | 377013439 |
P-2400 | 377013150 | 377013152 | 377013154 | 377013156 |
P-4000 | 377013151 | 377013153 | 377013155 | 377013157 |
LIJAS ABRASIVAS NO ADHESIVAS PARA PRE-PULIDO
Diámetros disponibles: Ø 200/230/250/300 mm
Cajas de 100 ud.
Papel abrasivo fijación no adhesiva
Granulometría: P-60 hasta P-4000
Utilización en materiales metálicos blandos ferrosos
Tipo de abrasivo: S (alúmina) o M (carburo de silicio)
- Para más información consulte la Tabla de Referencias
Opciones disponibles:
BANCO DE CALIBRACION ALESTA N 300 | 377013154, 377013155, 377013420, 377013421, 377013422, 377013423, 377013424, 377013425, 377013426, 377013427, 377013428, 377013429 |
---|---|
Descripción | P/100 Lijas Abra NA M 250 P-1000, P/100 Lijas Abra NA M 250 P-120, P/100 Lijas Abra NA M 250 P-1200, P/100 Lijas Abra NA M 250 P-180, P/100 Lijas Abra NA M 250 P-240, P/100 Lijas Abra NA M 250 P-2400, P/100 Lijas Abra NA M 250 P-320, P/100 Lijas Abra NA M 250 P-400, P/100 Lijas Abra NA M 250 P-4000, P/100 Lijas Abra NA M 250 P-600, P/100 Lijas Abra NA M 250 P-80, P/100 Lijas Abra NA M 250 P-800 |